Glass Fibres And Materials Made From Them

A boron-free alkali-free glass fibre with better fundamental properties than "E" fibre was developed. The process properties of the new glass allow drawing the glass fibre on existing equipment. The fibre is recommended for use as a filler for high-strength fibreglass-reinforced plastics and for reinforcing corrosion-resistant fibreglass-reinforced plastics.