Glass Fibre Reinforced, Sprayed Coating For Sealing Thermal Insulation Containing Asbestos

A novel method of sealing asbestos insulation has been developed. It consists of simultaneously spraying short glass fibre rovings and certain water based paints of the type commonly used for sealing asbestos such that the two components mix and form, when dry, a tough membrane reinforced with randomly oriented fibres.