Glass Dielectric Prepared By Two-Step Toughening

This article details a study that investigated the possibility to enhance the mechanical and thermomechanical performance of glass dielectrics by two-step toughening, short-term ion-exchange following thermal toughening.

Author
H Yoshimura & S Guedes
Origin
Fed University Abc & Prismatic Vidros, Brazil
Journal Title
Glass International July-August 2010 22-24, 25