Glass Decoloration - Radiation Colouration Of Glass - State-Of-The-Art

Slowly, but with a steadily increasing rate, studies have appeared on the processes occurring during the radiation of inorganic glasses, particularly on the structure of various colour centres and on the mechanism of their formation and decomposition. It is obvious that these studies required experiments with glasses of the simplest possible composition to simplify the complexity of these processes, and to make the interpretation easier. For this reason, a large number of studies were made with pure crystalline quartz and fused silica.

Author
Z Prasil & T Marlind
Origin
Dept Radiation Technology, Prague & Scan Caric, Sweden
Journal Title
Beta-Gamma 4/91 11-12
Sector
Primary Papers
Class
PP 90

Request article (free for British Glass members)

Glass Decoloration - Radiation Colouration Of Glass - State-Of-The-Art
Beta-Gamma 4/91 11-12
PP 90
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.