Glass Coating - The Key To Glass Production

One of the most successful treatments for improving glass strength has been the deposition of an extremely thin layer of tin oxide on the glass surface. In combination with a cold-end coating, a scratch-resistant and lubricious surface of the glass containers is created.

Author
E Van Wijk
Origin
Elna International
Journal Title
Total-Kleenmold.com/Wp-Content/Plugins/Google.../Load.Php?D...Pdf‎
Sector
Container glass
Class
C 5106

Request article (free for British Glass members)

Glass Coating - The Key To Glass Production
Total-Kleenmold.com/Wp-Content/Plugins/Google.../Load.Php?D...Pdf‎
C 5106
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.