Glass Ceramics In The System Diopside-Anorthite-Orthoclase Prepared By Using Some Industrial Waste Materials

Crystallisation of glasses based on the diopside anorthite eutectic system containing increasing amounts (0-30wt%) of orthoclase was studied.