Glass-Ceramics Prepared From Spodumene Mineral

The viability of fabricating lithium aluminosilicate (LAS) glasses and glass-ceramics from a naturally occurring spodumene mineral has been investigated. A deposit of spodumene (Li20.Al203.4Si02) obtained from Greenbushes, W Australia, has successfully been used to produce a transparent colourless glass. The experimental results have shown great potential of producing the LAS glass-ceramics using the more economical materials.

Author
A Nordmann & Yi-Bing Cheng
Origin
Monash University, Melbourne, Australia
Journal Title
Xvii Int Cong Glass, Beijing, October, 1995 Vol 6, 45-50
Sector
Glass Ceramics
Class
GC 301

Request article (free for British Glass members)

Glass-Ceramics Prepared From Spodumene Mineral
Xvii Int Cong Glass, Beijing, October, 1995 Vol 6, 45-50
GC 301
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.