Glass-Ceramics: Engineering Principles And Applications

The history and typical achievements in the development of glass-ceramics are reviewed on the basis of the engineering principles of crystallization in glass and its application. Bulk and surface crystallization phenomena and their practical applications are described as well as the forming process of glass ceramics. In addition to conventional glass ceramic materials and processes, novel potentialities of glass ceramics in next-generation devices are also indicated.

Author
A Sakamoto & S Yamamoto
Origin
Nippon Electric Glass, Japan
Journal Title
Int J Appl Glass Sci 1 3 2010 237-247
Sector
Glass Ceramics
Class
GC 738

Request article (free for British Glass members)

Glass-Ceramics: Engineering Principles And Applications
Int J Appl Glass Sci 1 3 2010 237-247
GC 738
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.