Glass-Ceramics Based On Calcium Phosphates - Artificial Dental Crown And Microporous Glass-Ceramics

Crystallization of calcium phosphate glasses and the derived glass-ceramics which have been investigated by us are briefly reviewed. The glass-ceramics containing an amount of Al2O3 are developed for artificial dental crowns which were prepared by a lost-wax technique. The glass-ceramics containing TiO2 (pseudo-binary system of RTi2(PO4)3-Ca3(PO4)2 ; R=Li, Na, 1/2Ca) were produced by bulk-crystallization of the glasses; the acid leaching of these glass-ceramics results in development of microporous glass-ceramics with a skeleton of NASICON-type titanium phosphate crystals.

Author
Y Abe
Origin
Chuba University, Japan
Journal Title
Glastech Ber Glass Sci & Technol 73 C1 2000 286-292
Sector
Glass Ceramics
Class
GC 805

Request article (free for British Glass members)

Glass-Ceramics Based On Calcium Phosphates - Artificial Dental Crown And Microporous Glass-Ceramics
Glastech Ber Glass Sci & Technol 73 C1 2000 286-292
GC 805
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.