Glass-Ceramic Technology - A Comprehensive New Book

The authors of Glass-Ceramic Technology make an informative contribution to those who want to know more about new glass-ceramic materials and their scientific/technological background or who want to use these materials and benefit from them. A good book for students, scientists, engineers and technicians which also serves as a reference for all those interested in natural or medical science and technology, with special emphasis on glass-ceramics as new materials with new properties. The first three chapters, "Principles of Designing Glass-Ceramic Formation," "Composition Systems for Glass-Ceramics" and "Microstructural Control," satisfy the requirements of a scientific-technological textbook. Further details on the book, and how to buy it can be seen on the website: www.ceramics.org

Author
W Holand & G Beall
Origin
Unknown
Journal Title
Am Ceram Soc Bull 81 4 2002 31-35
Sector
Glass Ceramics
Class
GC 452

Request article (free for British Glass members)

Glass-Ceramic Technology - A Comprehensive New Book
Am Ceram Soc Bull 81 4 2002 31-35
GC 452
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.