Glass-Ceramic Protective Coating For Titanium Alloys

A glass-ceramic coating that protects a titanium alloy against oxidation during heat treatment has been successfully developed. In this study, the conditions for preparing this glass-ceramic coating were investigated. In addition, the prepared coating was characterized by X-ray diffractometry, energy-dispersive spectroscopy analysis, and oxygen weight-gain testing. The results showed that the glass-ceramic coating has excellent oxygen-proof properties to protect the titanium alloy from oxidation by the atmosphere at high temperatures.

Author
L Wang Et Al
Origin
Dalian University, China
Journal Title
J Am Ceram Soc 85 11 2002 2867-2869
Sector
Glass Ceramics
Class
GC 491

Request article (free for British Glass members)

Glass-Ceramic Protective Coating For Titanium Alloys
J Am Ceram Soc 85 11 2002 2867-2869
GC 491
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.