Glass-Ceramic Foams From Borosilicate Glass Waste

This study reports of the work on a glass-ceramic foam with wollastonite and cristobalite micrometric crystals prepared by sintering a borosilicate glass waste with organic binder as foaming agent. The waste glass, coming from the dismantling of washing machine, was characterized by high CaO content and low-temperature sinterability. The effect of the temperature on the sinter-crystallization ability of the borosilicate glass waste was followed with thermal analysis, heating microscopy, and electron scanning microscopy (ESEM) observations. Additionally, the effect of temperature on the evolution of crystalline phases and density variation was monitored with XRD and density measurements. The softening started at 800 deg C and crystallization at 845 deg C to be completed at 900 deg C with a linear expansion of 38-40% in the range 850-900 deg C. Wollastonite and cristobalite were identified as crystalline phases in variable proportions dependently upon temperature. No crack evidence was found at high ESEM magnification even though cristobalite crystals were present. The final products showed a total porsity of around 78-79% and an apparent density of about 0.5g/cm3, in line with common porous closed cell glass foams used for thermal insulation.

Author
R Taurino Et Al
Origin
University Modena, Italy
Journal Title
Int J Appl Glass Sci 5 2 June 2014 136-145
Sector
Glass Ceramics
Class
GC 855

Request article (free for British Glass members)

Glass-Ceramic Foams From Borosilicate Glass Waste
Int J Appl Glass Sci 5 2 June 2014 136-145
GC 855
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.