Glass Ceramic Enamels With Increased Conductivity

Based on crystallizing alkaline boron-titanium-silicate glasses with oxide additives of the R2O type, ground and cover chemically stable enamels for steel have been developed, which exhibit high chemical resistance and high electrical conductivity.