Glass Bowls Made On The Potter'S Wheel. A New Approach To Ancient Glass Technology

The experimental reproduction of the technique of spirally wound reticella thread bowls (3rd century BC to first half 1st century AD) is described.

Author
R Lierke
Origin
Unknown
Journal Title
Glastech Ber 1991 64 12 310 - 317