Glass Armor - An Overview

Transparent armor for military vehicles has recently gained renewed attention. However, the ballistic impact and penetration processes of glass armors are not well understood. Different types of glasses exhibit different ballistic responses, and a pressing need exists to better comprehend and model these responses in order to develop lightweight armors. The need to better understand the processes of densification and dynamic fracture and the need for input and validation data for continuum models are highlighted as examples.

Author
T G Talladay & D W Templeton
Origin
Us Army Tank-Automotive Research, Warren, Michigan, Usa
Journal Title
Int J Appl Glass Sci 5 4 2014 331-333
Sector
Special Glass
Class
S 4156

Request article (free for British Glass members)

Glass Armor - An Overview
Int J Appl Glass Sci 5 4 2014 331-333
S 4156
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.