Glass Annealing And Method

The method of determining the degree of anneal or compacting of a piece of glass of a known composition comprising subjecting the piece of glass and a test piece of glass of substantially the same composition but of a known maximum index of refraction when completely annealed or compacted to an annealing cycle, determining the index of refraction of the test piece after passing through the annealing cycle to determine its degree of anneal or compacting by comparing the index of refraction of the test piece at the com.

Author
Ed Tillyer And Jw Ford
Origin
Unknown
Journal Title
American Optical Co. U.S 2,369, 189, Feb 1945
Sector
Primary Papers
Class
PP 1438

Request article (free for British Glass members)

Glass Annealing And Method
American Optical Co. U.S 2,369, 189, Feb 1945
PP 1438
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 18 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.