Glass And Ceramic Packaging: Food Contact Compliance (In Italian)

Glass and ceramics are the main materials used in contact with food and they are widely used as food containers (as bottles and jars), tableware (plates, cups, bowls etc.) and utensils for cooking. This paper aims to provide an indication of the main technical standards governing the sector in order to furnish an useful guide for manufacturers and users of glassware and ceramics for food use.

Author
Un-named
Origin
Unknown
Journal Title
Riv Staz Sper Vetro 43 2013 3 5-10 www.Spevetro.It/Archiviorssv/Rssv%203%202013.Pdf
Sector
Container glass
Class
C 4935

Request article (free for British Glass members)

Glass And Ceramic Packaging: Food Contact Compliance (In Italian)
Riv Staz Sper Vetro 43 2013 3 5-10 www.Spevetro.It/Archiviorssv/Rssv%203%202013.Pdf
C 4935
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.