Glass & Aluminium Bodies Reject Pet Study

FEVE & the EAA strongly questioned the use of the LCA methodology in research sponsored by PETRA. Both said the method employed for the PET body research is not designed to produce a carbon footprint comparison between packaging materials. The cradle-to-grave study, conducted by Franklin Associates for PETRA, compared total energy, solid waste & greenhouse gas emissions per/100,000-oz soft drinks packaged in 20-oz PET bottles, 8-oz glass bottles, or 12-oz aluminium cans. Results claimed PET bottles outperform aluminium can & glass bottles in terms of environmental footprint by using less energy, & creating significantly fewer greenhouse gases. FEVE's director challenged the validity of using the LCA method: "Comparative studies are dependent upon such a huge number of assumptions, that it is difficult to compare like with like & come to fair conclusions, to say the least."

Author
Un-named
Origin
Unknown
Journal Title
www.Foodproductiondaily.com 8 April 2010
Sector
Container glass
Class
C 4098

Request article (free for British Glass members)

Glass & Aluminium Bodies Reject Pet Study
www.Foodproductiondaily.com 8 April 2010
C 4098
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.