German-Japanese Link-Up For Prefillable Syringes

According to Euwid Verpackung, Bunder Glas, a subsidiary of Gerresheimer Glas, has signed an agreement with Taisei Kako, a manufacturer of packaging and application systems for the cosmetics and pharmaceutical industries in Japan. Through the new agreement, the successful cooperation between the two companies in marketing and manufacturing is to be extended to includeprefillable disposable syringes, highlighting the German company's commitment to meet the needs of the pharmaceutical industry.