Geometry Of Fused Cast Azs Palisade Blocks

Refel, founded in 1986, specialises in the manufacture of fused cast materials of the AZS system, used in all areas of glass furnace construction. In this paper the company discusses the importance of proper geometry for palisade blocks in order to conserve the life of the furnace and achieve high performance.