General Chemical To Idle 0.5M/Tpa Soda-Ash Plant

General Chemical Group Inc. (GCG) plans to idle 500,000 tpa of synthetic soda ash capacity at its Amherstburg, Ontario facility to improve operating efficiencies, generate cost savings and better utilise capital. The Hampton, new Hampsire-based company will complete the shutdown by 31 March 2001. Its customers will be served from its natural soda ash facility in Green River, Wyoming. The shutdown will remove about 15% of the company's total soda ash production capacity - all its Amherstburg production - leaving it with annual capacity of roughly 2.8m tpa in Green River.

Author
Un-named
Origin
Unknown
Journal Title
Industrial Minerals 400 January 2001 9
Sector
General
Class
G 2325

Request article (free for British Glass members)

General Chemical To Idle 0.5M/Tpa Soda-Ash Plant
Industrial Minerals 400 January 2001 9
G 2325
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.