Gas Technology In Glass Manufacturing - Ngc'S Venture Bears Fruit

During 1990, Nordic Gas Technology Centre (NGC) investigated the use of energy in the Nordic glass industry. The total energy consumption was found to be 2.5 TWh/year, of which the main part was in the area of the existing or planned natural gas grid. NGC then decided to start a research program on gas utilisation in the glass industry. The program was divided into three parts according to the types of products manufactured and types of furnaces used: art glass; container and sheet glass; and fibre glass and mineral wool.

Author
I Gunnarsson
Origin
Energi-Analys Ab, Sweden
Journal Title
Glasteknisk Tidskrift 49 2 1994 65-69
Sector
General
Class
G 1250

Request article (free for British Glass members)

Gas Technology In Glass Manufacturing - Ngc'S Venture Bears Fruit
Glasteknisk Tidskrift 49 2 1994 65-69
G 1250
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.