Gas Chromatographic Analysis Of Bubbles In Glass. (In English)

A gas chromatograph capable of analysing CO2, O2, N2, H2S, SO2 and CO within 25 minutes is described. The apparatus can determine the contents of bubbles down to 0.5mm in diameter.

Author
I Makino
Origin
Unknown
Journal Title
Reports Of The Asahi Glass Co 23 1 1973 1-7
Sector
Primary Papers
Class
PP 1284

Request article (free for British Glass members)

Gas Chromatographic Analysis Of Bubbles In Glass. (In English)
Reports Of The Asahi Glass Co 23 1 1973 1-7
PP 1284