[Furnaces] 3-In-1 Approach To Dust, Sox And Nox

This article discusses how the Ecopoure CCF, a new combined DeDust, DeSOx and DeNox process, has been used by a Chinese glassware manufacturer to combat excess emissions from its furnace. The technology means the glass maker can confidently face today's emission targets, as well as stricter goals that will be introduced in the future.