Furnace Redesign Brings Energy Savings In Tunisia

AGMS of Blaringhem, France, has successfully commissioned a 30/tpd soda lime glass furnace in Tunisia for Univer. Charged with improving the design of an existing installation, AGMS has enlarged and redesigned the furnace to reduce energy consumption and increase the specific full pull rate. The AGMS team of 100 specialists strives constantly for the best technical solutions, combining competitiveness and quality in the exercise of engineering projects and furnace repairs. The organisation's goal is to be a supplier of customised solutions from batching through gob forming.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide Nov-Dec 2011 16
Sector
General
Class
G 3930

Request article (free for British Glass members)

Furnace Redesign Brings Energy Savings In Tunisia
Glass Worldwide Nov-Dec 2011 16
G 3930
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.