Furnace Innovation For Nuclear Waste Vitrification.. And Much More

Years of technical development are coming to fruition at USA-based Stir-Melter, a wholly-owned subsidiary of Glasstech Inc. Stir-Melter recently signed a multi-million dollar contract with the US Department of Energy for a unit that will be used in a programme for the disposal of high level nuclear wastes. This full size prototype will be used by the Westinghouse Savannah River Co.