The Furnace Of The Future?

Glassmakers face increased environmental pressure over their emissions during the manufacturing process. Consumer trends and legislation dictate that emissions must be as low as possible. This article looks at some of the options for glassmakers when they choose their next furnace.

Author
Dr H Hegeler
Origin
Sorg, Germany
Journal Title
Glass International November 2019 21-22
Sector
General
Class
G 4769