Furnace Design And Equipment For Extended Furnace Life

Horn Glass Industries AG is one of the leading designers of glass melting furnaces and manufacturers of equipment for the glass industry. The company has over 130 years of longstanding experience and can provide excellent references. In this article, the author discusses a project for a client in India to design one of the world's largest (650/tpd capacity) end-fired furnaces.

Author
C Jatzwauk
Origin
Horn, Germany
Journal Title
Glass Worldwide Nov-Dec 2017 106-109