Fundamental Studies On Glass Melting Tanks. 1. Model Experiments On The Flow Of Gases In An End-Port Tank Using Water And Hot Gases As The Fuids.

Experiments with a two-dimensional model and water and alos a three-dimensional model and gases of a medium temperature.

Author
K. Terada And M. Wakamatsu
Origin
Unknown
Journal Title
Yogyo Kyokai Shi, 67, 61, 1959 (In Japanese)