All phenomena occurring in a glass tank furnace, i.e. melting the batch, refining and conditioning the molten glass, and other chemical and physical processes, are connected inseparably with the convection currents of molten glass. It may, therefore, be said that the effort to understand these complicated processes cannot be successful without learning the fundamental characteristics or trends of convection currents.

Author
K Takahashi & C Higashi
Origin
Unknown
Journal Title
J Ceram Assoc Japan 67 765 1959 301-311
Sector
Primary Papers
Class
PP 135

Request article (free for British Glass members)

Fundamental Studies On The Characteristics Of Convection Currents Of Molten Glass By Model Techniques
J Ceram Assoc Japan 67 765 1959 301-311
PP 135
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.