Fullerenes Entrapped In Porous Glass

Fullerenes have been impregnated in porous glass with little interaction with the glass noted. Concentrations as high as 3mg/ml of C60 or C70 were obtained. It was shown that the fullerenes can enhance the photo-induced charge transfer reaction of DEA with the porous glass.

Author
N F Borrelli Et Al
Origin
Corning Inc, Ny, Usa
Journal Title
Corning Research 1994 57-64