Considering advantages due to the oxide composition, energy content of the glass and ecological effects, usage in frits and glazes of E-glass fibre waste represents an important reason for their study. The main purpose of this paper is to present the results of experiments concerning E-glass fibre waste containing around 7% B2O3 for obtaining glazes for tableware ceramics, as well as to study the consequences upon fabrication technology.