Friction Behaviour Of Hot Glass On Metal Surfaces

Friction experiments between hot television glass and a commercial 13% Cr-steel, uncoated and coated with Cr and NiW have been performed with a pressing-friction apparatus on a laboratory scale. Also, the influence and friction reducing effects of several commercial lubricants have been studied. The results showed that friction coefficients measured at contact temperatures above 540 deg C, which is about 80 deg C below sticking temperature, already start increasing sharply. For NiW the lowest friction coefficients were obtained. The effective life-time of the lubricants has been tested as a funciton of the number of pressing-friction cycles.

Author
N M Keulen & M G F C Sanders
Origin
Philips Components Bv, Netherlands
Journal Title
Ceramic Trans 82 1998 257-262
Sector
Special Glass
Class
S 1615

Request article (free for British Glass members)

Friction Behaviour Of Hot Glass On Metal Surfaces
Ceramic Trans 82 1998 257-262
S 1615
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.