Frequency And Temperature Dependent Dielectric Properties Of Greentapes

Investigation into the fabrication of dielectric materials suitable for low temperature co-fired ceramic (LTCC) applications and their characterisation at high frequencies is a prominent research area. There re only limited reports presenting microwave properties of material before firing takes place. This paper reports the dielectric properties of the GreenTapes at low frequencies and at microwave frequencies. Low and High frequency dielectric properties of greentape material at room temperature are studied using a LCR meter and dielectric probe technique respectively. Split post dielectric resonator technique is used in the temperature range from 10K to 290K for the estimation of complex permittivity.

Author
M V Jacob Et Al
Origin
James Cook University, Queensland, Australia
Journal Title
J Aust Ceram Soc 46 1 2010 36-40
Sector
Glass Ceramics
Class
GC 725

Request article (free for British Glass members)

Frequency And Temperature Dependent Dielectric Properties Of Greentapes
J Aust Ceram Soc 46 1 2010 36-40
GC 725