Fragmentation Of Glass Bottles By Impact

Three sizes of water-filled generic soft-drink containers were impacted against a blunt steel rod striking the middle sidewall. The fracture origins of the containers were in hinge breaks. The containers showed a linear relation between the number of primary cracks and the energy of impact.