Fractography Of Glasses And Glass Ceramic Materials (Spanish)

The fracture and fracture analysis of glasses and ceramics are discussed with reference to the effects of composition and microstructure. Fractography of vitreous materials is compared with that of ceramics and metals.

Author
J Ma Rincon, P Callejas, F Capel
Origin
Instituto De Ceramica Y Vidrio
Journal Title
Bol Soc Esp Ceram Vidr 1989 28 4 257-267