Forming Solutions For The Narrow Neck Press And Blow Process

The NNPB process provides the greatest possibility for lightweighting narrow neck containers. By mechanically forming the parison, glass distribution is control and the result is a finished container with a more even wall thickness. Compared to the conventional blow-blow process, manufactures can achieve a final product that is around 30% lighter. This article outlines a number of solutions to overcome the problems associated with the NNPB process.