[Forming] Individually Adjustable Cooling Of Glass Containers

In this article, the author explains how IS machine manufacturer GPS has obtained a patent for a recently developed wind box.

Author
R Themann
Origin
Gps Glasproduktions-Service, Germany
Journal Title
Glass Worldwide March-April 2017 58-59