[Forming] High Speed Vial Production Expertise

According to the author of this article, OCMI vial forming machines increase productivity thanks to their employment of continuous rotation, without losing accuracy in subsequent processing.

Author
A Crescentini
Origin
Ocmi, Italy
Journal Title
Glass Worldwide Jan-Feb 2015 66-67
Sector
Container glass
Class
C 5377

Request article (free for British Glass members)

[Forming] High Speed Vial Production Expertise
Glass Worldwide Jan-Feb 2015 66-67
C 5377
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 14 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.