The characteristics of an Al203 coating on a Nb or Mo substrate using a direct current-radio frequency induction thermal plasma of Ar-H2 were studied. A porous and crystallographically stable coating with highly preferred orientation of [110] planes of x-Al203 crystals was obtained. The preferred orientation was strongly dependent on the diameter of the introduced Al203 powder. The formation mechanism of the preferred orientation of the coating is explained by accumulation of charged clusters on the substrate. The coating prepared by this procedure revealed the superior capability of protecting the substrate against high-temperature oxidation.

Author
A Otsuka Et Al
Origin
Japan Ultra High Temp Research Inst
Journal Title
Jacs 86 7 2003 1068-1075
Sector
Special Glass
Class
S 2541

Request article (free for British Glass members)

Formation Of An Environmental Barrier Coating Using Dc-Rf Hybrid Plasma
Jacs 86 7 2003 1068-1075
S 2541
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.