Formation Of Barrier Ribs For Plasma Display Panels Via Powder-Blasting Process: Part Ii Effects Of Powder-Blasting Angle

The effects of powder-blasting angle on the powder-blasting rate of a thick film prepared using a tape-casting technique ave been investigated. The results reveal that the etching rate was sensitive to the angle of powder blasting. The mechanism of this dependency was discussed based on brittle fracture and erosion caused by the powders blasted on the surface of the film. In addition, a new processing route for barrier ribs for plasma display panels was attempted, using the sensitive dependency of the etching characteristics on the powder-blasting angle. It was demonstrated that the ribs could be processed successfully using layers having different etching rates.

Author
Y Kim Et Al
Origin
Hongik University, Seoul, Korea
Journal Title
J Am Ceram Soc 87 3 2004 348-351
Sector
Special Glass
Class
S 2774

Request article (free for British Glass members)

Formation Of Barrier Ribs For Plasma Display Panels Via Powder-Blasting Process: Part Ii Effects Of Powder-Blasting Angle
J Am Ceram Soc 87 3 2004 348-351
S 2774
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.