Formation And Properties Of Sodium Scandium Silicate Glasses

Sodium scandium silicate glasses can be formed containing a maximum of approximately 15 mol% Sc203. The addition of scandium oxide to these glasses increases their density, refractive index and glass transformation temperature.

Author
J E Shelby & J J Noonan
Origin
Alfred University, New York
Journal Title
Phys Chem Glasses 38 5 1997 251-255
Sector
Special Glass
Class
S 1238