Formation And Properties Of Soda Lime Aluminate Glasses

Glasses containing 0-10mol% soda, 50-70mol% CaO, and 30-44mol% alumina can be produced in the soda lime aluminate system. The glass forming ability in this system is relatively independent of soda content until it decreases rapidly near 10mol% soda. Crystallisation of glasses containing