[Food Contact/Plastics] Commission Directive Adopted

The Commission has adopted the 5th amendment of Directive 2002/72/EC relating to plastic materials and articles intended to come into contact with food. The Directive establishes lists of authorised substances for the manufacture of these materials and articles, in particular additives and monomers, restrictions on their use, as well as rules on labelling and onto he information to be given to consumers or food business operators for the correct use of these materials and articles. The current list of additives contained in the Directive is an incomplete list inasmuch as it does not contain all substances currently adopted in one or more Member States.

Author
Un-named
Origin
Unknown
Journal Title
Cpiv News March 2008
Sector
Container glass
Class
C 3644

Request article (free for British Glass members)

[Food Contact/Plastics] Commission Directive Adopted
Cpiv News March 2008
C 3644
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
11 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.