Foaming Behaviour On Glass Melts

State-of-the-art of foam stability is presented which focuses on specific problems in glass melts. The experimental part offers three measuring methods for the quantitative evaluation of foaming behaviour on glass melts: the direct observation of foam decay; stability investigations on single lamellae, and life time measurements of single bubbles, in all cases as functions of various parameters such as temperature and composition of the furnace atmosphere. Experimental findings demonstrate that foam decay on glass melts occurs through the sequence of a drainage and a tear process. Probably the tearing of lamellae at the foam surface is rate determining. A general theory of foam stability cannot yet be developed at this time, however, some recommendations for plant practice can be derived from the results.

Author
J Kappel Et Al
Origin
Fraunhofer Inst, Germany
Journal Title
Glastech Ber 60 6 1987 189-201
Sector
Special Glass
Class
S 2561

Request article (free for British Glass members)

Foaming Behaviour On Glass Melts
Glastech Ber 60 6 1987 189-201
S 2561
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.