Fluoroberyllate Glasses Of The System Bef2-Kf-Aif3-Yf3

These glasses are stable with respect to crystallisation and are moisture resistant.

Author
G.P. Nikolina Et Al.
Origin
Unknown
Journal Title
Izv. Akad. Nauk Sssr Neorg. Mater., 7 [3] 527-29 (1971)
Sector
Primary Papers
Class
PP 923