Fluoride Glasses Of 3D Transition Metals

Large vitreous areas have been found in PbF-MF2-MF3 systems (M=3d transitional element). The chemical and thermal conditions of preparation are given. These glasses exhibit interesting physical properties: good infrared transparency up to 7.5nm for 3mm thickness,luminescence with rare garth ions, and spin glass behaviour for high Mn2+/Fe3+ content.

Author
C. Jacoboni Et Al.
Origin
Unknown
Journal Title
Glass Technology 1983 24 (3) 164-7