Fluoride Analysis Of Glasses And Silicate Materials By Pyrohydrolosys Seperation

Fluoride in a wide variety of glasses and silicate materials can be separated by pyrohydrolosis and then determined by titration with Th. Pyrohydrolosis is accomplished is accomplished by passing steam over a mixture of sample and U3O8 at temperatures of approximately 1,000C.

Author
P.B. Adams. J.P. Williams.
Origin
Unknown
Journal Title
J. Amer. Ceram. Soc., 41, 377, 1958