Fluid Dynamics Analysis Leading To Innovative Glass Homogenization Device "Arctwister"

The quality of the glass melt is determined by thermal and compositional homogeneity across the feeding channel. Achieving that homogeneity with stirrers made from precious metals as well as from refractory is a widespread method used in the glass industry. Homogenization of glass melts by stirring happens under laminar flow conditions due to the low Reynolds-numbers at typical stirring temperatures and viscosities. As the glass viscosity conditions do not permit turbulence, good homogenization is hard to achieve. Compositional and thermal differences such as cords cannot be fully dispersed, they can only be stretched and folded until they are virtually invisible. This poses the question what stirrer geometry is fluid-dynamically efficient, as well as considering a multitude of other requirements such as low precious metal weight, longevity and robustness. In a project carried out by Umicore Platinum Engineered Materials, the flow inside a stirring cell was studied by computational fluid dynamics and predominantly by physical simulation in order to develop an advancing stirring device. Cord was simulated by coloured tracer liquid at different locations in a glucose model and different stirring concepts were tested and compared. The exercise revealed valuable insight into hwo the glass flow should be affected and what geometry an efficient stirrer should have when it can be made from oxide dispersion strengthened PtRh-alloy. Finally, the study led to the development of the ARCtwister, a modular, self-supporting stirrer made from fine grain stabilized FKS-PtRh-alloy. The stirrer creates a unique S-curved flow characteristic moving the glass volume vertically. It also transports the glass horizontally from the outside to the bowl centre and vice-versa. This concept provides very efficient homogenization, even at low speeds. Its combination of stiff stirring members, tubes, arcuated blades and helices creates an extremely rigid framework allowing for thin precious metal wall thicknesses.

Author
A Fuchs
Origin
Umicore Ag, Germany
Journal Title
77 Conference On Glass Problems 2017 131-141
Sector
General
Class
G 4616

Request article (free for British Glass members)

Fluid Dynamics Analysis Leading To Innovative Glass Homogenization Device "Arctwister"
77 Conference On Glass Problems 2017 131-141
G 4616
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.