Flue Gas Treatment And Electricity Generation

In this article, the author considers the potential for heat recovery and energy generation from glass furnaces, taking into account the different flue gas cleaning functions. An overview of traditional and the latest technical solutions for dedusting, deacidification, and deNOx operations is provided.